FIELD: inorganic chemistry. SUBSTANCE: pulp of origin halenite in neutral 20-25% solution of sodium or potassium chloride is prepared. Said solution contains polyacrylamide, its quantity being 0.1-0.3 mg/l, mass ratio of solid and liquid phases being (2-4): 1. Then electrolysis is carried out by uninterrupted draining off upper layer of solution thus prepared hydroxide. The process takes place to isolate hydroxide and to remove mother solution for production fresh portions of pulp. EFFECT: increases desired product yield, decreases expense of its production. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF REFINING LOW-MELTING METALS | 1991 |
|
RU1776093C |
0 |
|
SU462442A1 | |
0 |
|
SU510857A1 | |
0 |
|
SU538063A1 | |
METHOD FOR PRODUCING HIGH-PURITY LITHIUM HYDROXIDE MONOHYDRATE FROM MATERIALS CONTAINING LITHIUM CARBONATE OR LITHIUM CHLORIDE | 2019 |
|
RU2751710C2 |
PROCEDURE FOR PREPARING WATER SOLUTION OF REAGENTS FOR LEACHING METALS FROM ORE MINERAL STOCK | 2009 |
|
RU2413013C1 |
METHOD OF OBTAINING THE ANTIMONY POWDER | 1991 |
|
RU1804030C |
METHOD OF OBTAINING SODIUM CHLORINEOXYGEN SALT | 0 |
|
SU672222A1 |
METHOD OF PRODUCTION OF HIGH-PURITY LITHIUM HYDROXIDE FROM NATURAL BRINES | 1998 |
|
RU2157338C2 |
METHOD OF ELECTROLYTIC SEPARATION OF LEAD BISMUTHIDE | 0 |
|
SU701178A1 |
Authors
Dates
1994-01-30—Published
1991-06-27—Filed