FIELD: oil production. SUBSTANCE: portland cement for "cold" wells is mixed with water in proportion 1.0-1.2. Prepared suspension is cured for 20-30 min and is then treated in disintegrator at particle collision speed of 25- 30 m/s. EFFECT: improved quality of grouting mortars.