FIELD: ferrous metallurgy technology. SUBSTANCE: sintering material is cooling at furnace top grill after grinding at temperature 900 C. Agglomerate is caking by sinter burden firing in blast regime. Carbon oxide of waste gas is firing by pure oxygen mixing by gas blasting. EFFECT: more effective processing. 1 dwg