FIELD: manufacture of artificial leather. SUBSTANCE: method involves forming face and adhesive polyurethane layers on backing from 25-% solution of polyurethane in dimethylformamide with 0.8-1.1 wt. -% of lithium chloride and 9.9-10.1 wt. -% of polyurethanesemicarbazide. Then said layers are doubled with cotton textile base. Said base is impregnated in advance with a solution of natural bischofite to its content in artificial leather reaching 60-70 wt. -% of dry matter. EFFECT: production of fire-resistant artificial leather. 3 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ARTIFICIAL LEATHER | 1998 |
|
RU2134737C1 |
ARTIFICIAL SKIN | 1998 |
|
RU2142030C1 |
SIMULATED LEATHER | 2006 |
|
RU2307208C1 |
BOOK-BINDING MATERIAL | 0 |
|
SU711221A1 |
FIREPROOF DECORATIVE-FINISHING MATERIAL AND METHOD OF OBTAINING THEREOF | 2012 |
|
RU2523330C2 |
BOOK BINDING MATERIAL | 0 |
|
SU926136A1 |
METHOD FOR TAR-WATER TREATMENT | 1994 |
|
RU2057083C1 |
HERMETIC ELASTIC MATERIAL | 2010 |
|
RU2443820C1 |
LIGHT-REFLECTING MATERIAL | 2002 |
|
RU2224059C1 |
SAND COMPOSITION FOR MAKING MOULDS AND CORES | 0 |
|
SU1159715A1 |
Authors
Dates
1994-04-15—Published
1992-01-09—Filed