FIELD: production of wood- fiber plates. SUBSTANCE: composition contains product of interaction of resol phenol-formaldehyde resin and saponified tallow oil at mass ratio (85-90):(10-15), paraffin, sulfuric acid and wood fiber. Ratio of mentioned above components, mass % is: 0.4-1.2, 0.5-1.0, 0.8-1.0 respectively. Wood fiber is mixed with sulfuric acid, paraffin and phenol binder. EFFECT: improves quality of desired product. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PRODUCTION OF MODIFIED PHENOL-FORMALDEHYDE RESIN | 1995 |
|
RU2100381C1 |
0 |
|
SU1778123A1 | |
GLUE COMPOSITION FOR WOOD-FIBER TILE | 2001 |
|
RU2213753C2 |
COMPOSITION FOR CHIP WOOD BOARDS | 0 |
|
SU1643575A1 |
BINDER FOR LOW-TOXIC WOOD PLASTIC MATERIALS | 1999 |
|
RU2162860C2 |
METHOD OF MODIFIED PHENOLFORMALDEHYDE RESIN PRODUCTION | 0 |
|
SU1786042A1 |
COMPOSITION FOR WOOD FIBER BOARDS | 2001 |
|
RU2196791C1 |
MIXTURE FOR PRODUCING WOOD FIBER BOARDS | 0 |
|
SU1707035A1 |
WOOD-FIBER MATERIAL, METHOD FOR PRODUCTION OF WOOD-FIBER MATERIAL AND METHOD FOR PRODUCTION OF BINDER FOR WOOD-FIBER MATERIAL | 1993 |
|
RU2076125C1 |
COMPOSITION FOR SOFT GROUNDWOOD BOARD | 2003 |
|
RU2245890C2 |
Authors
Dates
1994-07-15—Published
1989-03-30—Filed