FIELD: metallurgy. SUBSTANCE: 5.7-6.7 aluminium; 2.8-3.8 molybdenum; 0.7-1.65 tin; 0.7-1.65 zirconium; 0.1-0.3 silicon; 0.05-0.15 iron; 0.01-0.08 carbon; 0.005-0.04 nitrogen; 0.05-0.15 oxygen; and titanium, the balance, the Al+Sn+Zn+Si/Mo to Me ratio being 2.5-2.85. The claimed alloy is superior over that known in the art by at least 15 % in prolonged strength and a prolonged service life of 5000 hr, at least 10% in low-cyclic fatigue, and by 40% in crack resistance. EFFECT: improved properties of the alloy. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
TITANIUM-BASE ALLOY | 1996 |
|
RU2090642C1 |
TITANIUM-BASED ALLOY | 1996 |
|
RU2086695C1 |
TITANIUM-BASE ALLOY | 1992 |
|
RU2048572C1 |
WELDABLE TITANIUM-BASED ALLOY | 1996 |
|
RU2086694C1 |
TITANIUM-BASE HEAT RESISTANT ALLOY | 1992 |
|
RU2039112C1 |
TITANIUM BASED ALLOY AND PRODUCT MANUFACTURED THEREFROM | 2000 |
|
RU2175992C1 |
TITANIUM-BASE ALLOY | 1991 |
|
RU2030474C1 |
WELDABLE TITANIUM ALLOY EXHIBITING L-STRUCTURE | 1994 |
|
RU2082804C1 |
TITANIUM-BASE ALLOY | 1983 |
|
RU1131234C |
GRANULATED HIGH-TEMPERATURE NICKEL ALLOY AND PRODUCT MANUFACTURED THEREFROM | 2016 |
|
RU2623540C1 |
Authors
Dates
1994-07-15—Published
1992-07-20—Filed