FIELD: light industry. SUBSTANCE: method is carried out in two stages. At the first stage the leather waste with a liquid coefficient of 0.75-0.8 is treated by boiling for 15-20 min in an aqueous solution of sulfuric acid and NMK concentrate. At the second stage the reaction mass is boiled with stirring for 50-60 min and treated with a threefold amount of leather waste. Finally, the reaction mass is kept boiling for 3.0-4.0 h. EFFECT: production of highly-concentrated aqueous solutions of proteins with simultaneous reduction of consumption of chemicals and curtailing of the process. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF TANNING OUT OF COLLAGEN-CONTAINING WASTE OF CHROME TANNING FOR PROTEIN SUBSTANCE PREPARING | 0 |
|
SU1823879A3 |
METHOD FOR PROCESSING LEATHER INDUSTRY WASTES INTO FIRE-PROOF MATERIAL | 1991 |
|
RU2024616C1 |
METHOD OF LEATHER TREATMENT AND A METHOD OF POLYPEPTIDES PREPARING FOR LEATHER FILLING | 0 |
|
SU1838424A3 |
PROCESS OF TREATMENT OF HIDES | 0 |
|
SU1831501A3 |
METHOD OF DETANNING COLLAGEN-CONTAINING WASTE OF CHROME TANNAGE WITH OBTAINING PROTEIN SUBSTANCE | 0 |
|
SU1118656A1 |
METHOD OF PRODUCING PROTEIN HYDROLYSATE | 0 |
|
SU1733439A1 |
METHOD OF DETANNAGE OF LEATHER WASTE OF CHROME TANNAGE | 0 |
|
SU1822861A1 |
METHOD OF CHROME TANNING AGENT PREPARING | 1991 |
|
RU2017824C1 |
PROCESS FOR DETANNING COLLAGENACEOUS WASTES OF CHROMIUM TANNING | 0 |
|
SU994534A1 |
METHOD OF DETANNING COLLAGEN-CONTAINING WASTE OF CHROME TANNING | 0 |
|
SU1687591A1 |
Authors
Dates
1995-04-30—Published
1992-03-06—Filed