FIELD: manufacture of building materials and construction. SUBSTANCE: method for preparation of mortar and concrete mixes includes preliminary treatment of fine and coarse fillers with 0.005-0.1% aqueous solution, of nitrogen-containing inhibitors of acid corrosion of steel, particular C-5Y, and subsequent mixing with cement. Maximum increment of compression strength of concrete on modified fillers is 52% and cement consumption reduction by 15% EFFECT: higher efficiency. 2 cl, 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING MORTARS AND CONCRETE MIXES | 0 |
|
SU1328327A1 |
ADDITION FOR CONCRETE MIXTURE | 1993 |
|
RU2072971C1 |
METHOD OF PREPARING MORTAR | 0 |
|
SU1196347A1 |
METHOD OF PREPARING MORTAR | 0 |
|
SU1196354A1 |
METHOD OF FOAM CONCRETE MIXTURE PRODUCING | 1993 |
|
RU2064913C1 |
METHOD OF ACTIVATION OF FILLING AGENT AT CONCRETE MIXTURE MAKING | 1994 |
|
RU2087442C1 |
CONCRETE MIX | 2012 |
|
RU2515639C1 |
FINE-GRAINED CONCRETE MIXTURE AND PREPARATION METHOD THEREOF | 2012 |
|
RU2494061C1 |
METHOD FOR PREPARING MORTAR MIX | 0 |
|
SU1096250A1 |
METHOD FOR PRODUCTION OF SOLVENT MIXTURE | 1996 |
|
RU2111187C1 |
Authors
Dates
1995-07-20—Published
1992-03-03—Filed