FIELD: protective and decorative coatings. SUBSTANCE: composition has, varnished colloxylin 8.5-12.3; low-molecular butadiene nitrile rubber of molecular mass 18-20000 3.5-7.2; epoxy diane resin ЭД-20 1.5-2.5; butyl acetate 32.3-34.5; acetone 7.8-8.7, and toluene 40.5-40.7. Rubber and ЭД-20 were added to the colloxylin solution and stirred up to the complete homogeneity. Pigment, dye, filler can be added to the prepared composition. Properties: heat stability at 60 C, 55 min. adhesion to wood, 1 point, to metal, 2 points, bending film elasticity is 5-7 mm. EFFECT: enhanced quality of composition. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ADHESIVE COMPOSITION | 1993 |
|
RU2049801C1 |
METHOD OF PREPARING VARNISHED COMPOSITION | 1998 |
|
RU2134706C1 |
EPOXIDE COATING COMPOSITION | 1999 |
|
RU2180907C2 |
CONDUCTING DYE | 1994 |
|
RU2042694C1 |
POLYMERIC PROTECTIVE BARRIER COATING | 2006 |
|
RU2306325C1 |
THERMOPLASTIC COMPOSITION | 1997 |
|
RU2129134C1 |
PROTECTIVE COATING COMPOSITION | 2011 |
|
RU2480499C2 |
COMPOSITION FOR PROTECTIVE COVER | 2005 |
|
RU2290421C1 |
NAIL POLISH | 2001 |
|
RU2188625C1 |
HYDROINSULATING COMPOSITION FOR COATINGS | 1995 |
|
RU2086596C1 |
Authors
Dates
1995-11-10—Published
1992-12-29—Filed