FIELD: production of dyes. SUBSTANCE: waste solution of etching ferrum which contains copperas and sulfuric acid are neutralized by lime to pH 6.0-7.0. This process is carried out by blowing air. Thus prepared precipitate is filtered and washed by water within 3-3.5 h. Then calcination within 1 h at 750-800 C takes place. EFFECT: improves efficiency of method, simplifies the process. 1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| METHOD OF PRODUCING IRON-CALCIUM PIGMENT | 2010 |
|
RU2451706C1 |
| METHOD FOR PREPARING IRON AND CALCIUM PIGMENT | 0 |
|
SU1054389A1 |
| METHOD OF PRODUCING YELLOW IRON-CALCIUM PIGMENT | 0 |
|
SU1581727A1 |
| METHOD FOR PRODUCING IRON- AND MANGANESE-CONTAINING PIGMENTS FROM INDUSTRIAL WASTE | 2020 |
|
RU2756464C1 |
| METHOD OF OBTAINING IRON OXIDE PIGMENTS | 2017 |
|
RU2656047C1 |
| METHOD OF OBTAINING IRON OXIDE PIGMENTS | 2017 |
|
RU2655336C1 |
| METHOD OF PROCESSING SPENT SULPHURIC ACID ETCHING SOLUTIONS | 2020 |
|
RU2740063C1 |
| METHOD FOR PROCESSING SLURCHEN OF ACID MINE WATER | 2018 |
|
RU2690330C1 |
| PROCESS FOR PRODUCING IRON OXIDE PIGMENTS | 0 |
|
SU929669A1 |
| METHOD OF PREPARING FERRUM OXIDE | 0 |
|
SU1740320A1 |
Authors
Dates
1996-05-27—Published
1993-02-12—Filed