FIELD: metal coverings. SUBSTANCE: copper gas-thermal covering spray-coated on the steel substrate undergoes the rolling with compression to 15- 30% followed by keeping at the temperature 800-950 C under a reduction atmosphere for at least 5 min. EFFECT: new method proposed. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF TREATMENT OF FLAME-PLATED ALUMINUM COATS | 0 |
|
SU1731864A1 |
METHOD OF TREATMENT OF ALUMINUM COATS | 0 |
|
SU1730194A1 |
METHOD FOR PREPARING STEEL STRIP FOR MAKING ELECTRICALLY WELDED TUBES WITH CORROSION-PROOF COATING | 2002 |
|
RU2214877C1 |
METHOD OF GAS-THERMAL COATING PRODUCTION | 1994 |
|
RU2063470C1 |
PROCESS OF FOLLOWING TREATMENT OF SPRAYED-ON ALUMINIUM COATS | 1991 |
|
RU2006518C1 |
METHOD OF ROLLING STEEL STRIPS WITH SINGLE-SIDE GASOTHERMIC ALUMINIUM COATING | 0 |
|
SU1708453A1 |
METHOD FOR APPLICATION OF ALUMINIUM GAS-THERMAL COATING | 0 |
|
SU1791464A1 |
METHOD OF COMPACTING ALUMINUM COATING | 1992 |
|
RU2031971C1 |
METHOD OF PREPARATION OF STEEL STRIP FOR MOLDING TUBES WITH ANTIRUST COATING | 0 |
|
SU1807902A3 |
METHOD OF MAKING ALUMINUM-COATED STRIPS | 0 |
|
SU1750755A1 |
Authors
Dates
1996-07-10—Published
1993-05-25—Filed