FIELD: oil and gas well drilling. SUBSTANCE: cement is mixed with water comprising 0.21 - 0.33 % hypane as stabilizer for earlier tempering the cement stone. Stabilization of cement stone earlier tempering with 0.8 water/cement ratio in wells with up to 10 C temperature conditions. EFFECT: higher efficiency. 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD FOR PREPARING PLUGGING MIX | 0 |
|
SU935597A1 |
METHOD OF PREPARING LIGHT-WEIGHT GROUTING MORTAR | 1999 |
|
RU2162510C2 |
METHOD OF PREPARING PLUGGING SOLUTION | 1996 |
|
RU2106479C1 |
METHOD OF PREPARATION OF LIGHT GROUTING MORTAR OF DENSITY 1450-1500 kg/m | 2008 |
|
RU2385894C1 |
METHOD OF PREPARING BUFFER FLUID | 0 |
|
SU740933A1 |
SUPERLIGHTWEIGHT FOAM-CEMENT PLUGGING FLUID | 0 |
|
SU927973A1 |
COMPLEX STABILIZING REAGENT OF PLUGGING-BACK MUD | 0 |
|
SU1838585A3 |
BUFFER LIQUID | 0 |
|
SU1089101A1 |
PLUGGING COMPOSITION | 0 |
|
SU1451258A1 |
METHOD OF GROUTING MORTAR-PREPARATION | 2002 |
|
RU2213844C1 |
Authors
Dates
1997-01-20—Published
1992-04-13—Filed