FIELD: manufacture of leathers of different purpose. SUBSTANCE: amino compounds, acid collagen hydrolysate and formaldehyde. Process is carried out at temperatures of 18-23 C, for 1 or 2 hours, the ratio of components of the reaction mixture (wt%) being as follow: 20-30 amino compound: 40-60 acid collagen hydrolysate ; 20-30 formaldehyde. EFFECT: more efficient preparation process. 3 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARING SYNTHETIC TANNER | 1998 |
|
RU2129162C1 |
METHOD OF LEATHER WORKING | 1995 |
|
RU2083673C1 |
METHOD OF VEGETABLE TANNING AGENT PREPARING | 1997 |
|
RU2112041C1 |
METHOD OF PREPARING SYNTHETIC TANNER FOR CLEAR SKINS | 1999 |
|
RU2156305C1 |
METHOD OF PREPARING METAL-CONTAINING SYNTHETIC TANNER | 2002 |
|
RU2198223C1 |
METHOD OF MANUFACTURING LEATHER WITH TIGHTENED FACE SURFACE | 1999 |
|
RU2157410C1 |
METHOD OF SYNTHESIS OF SYNTHETIC TANNING AGENT | 1995 |
|
RU2091493C1 |
METHOD OF LEATHER TREATMENT | 2002 |
|
RU2193601C1 |
LEATHER MANUFACTURE PROCESS | 1998 |
|
RU2129164C1 |
METHOD OF WORKING OUT TANNED INTERMEDIATE PRODUCT | 1997 |
|
RU2107731C1 |
Authors
Dates
1997-07-27—Published
1995-11-16—Filed