FIELD: materials for furniture and interior finishing. SUBSTANCE: material consists of internal board and outside polymer coating manufactured by applying polymerizable composition including (in wt %): oligoesteracrylate, 30-40; mineral filler, 48-61; plasticizing additive, 3-10; photoinitiator, 1-10; and pigment, 0.01-1. The latter may be iron oxide, carbon black, phthalocyanine dyes or their mixture. Hardening of composition is initiated by UV radiation of mercury lamp with power at least 1 kW. Thickness of hardened coating is 1-2 mm. To extend color spectrum of dyed decorative material, polymerizable composition is supplemented by 0.01-5 wt % of a fat-soluble dye. Surface relief may be reduced by placing silicate glass sheet onto polymerizable composition prior to be UV irradiated. EFFECT: improved decorative quality of coating. 3 cl, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF MAKING DECORATIVE COATING | 2012 |
|
RU2515521C2 |
METHOD OF MANUFACTURE OF POLYMER LAMINATED MATERIALS | 1999 |
|
RU2147999C1 |
PHOTOPLYMERIZING DIELECTRIC COMPOSITION | 1990 |
|
RU2034886C1 |
ANAEROBIC HERMETIC COMPOSITION | 1991 |
|
RU2036947C1 |
ANAEROBIC HERMETIC COMPOSITION | 1991 |
|
RU2036946C1 |
ANAEROBIC COMPOSITION | 1992 |
|
RU2043385C1 |
ADHESIVE COMPOSITION FOR PRODUCING SILICATE TRIPLEXES | 1991 |
|
RU2007431C1 |
ADHESIVE COMPOSITION FOR MANUFACTURING OF SILICATE TRIPLEX | 1991 |
|
RU2043382C1 |
COMPOSITION FOR PREPARING CLEAR FRAGILE POLYMERIC MATERIAL | 1991 |
|
RU2050385C1 |
MULTILAYER COMPOSITION MATERIAL FOR BULLET-PROOF GLAZING | 1992 |
|
RU2057025C1 |
Authors
Dates
1998-03-10—Published
1996-04-03—Filed