HIGH-TEMPERATURE WROUGHT ALLOY Russian patent published in 1998 - IPC

Abstract RU 2107107 C1

FIELD: metallurgy; applicable in manufacture of high-temperature manifold-pipes of plants for production of ammonia, methanol and others with operating conditions conducted at temperature of 750-950 C and pressure up to 50 atm. SUBSTANCE: high-temperature wrought alloy contains components in the following quantities, wt.%: carbon 0.06-0.1; silicon within 0.7; manganese 0.7; chromium 19.0-23.0; nickel 30.0-34.0; titanium 0.25-0.80; aluminium within 0.5; sulfur within 0.02; phosphorus within 0.03; copper within 0.2; molybdenum within 0.5; lead within 0.01; tin within 0.01; arsenic within 0.01; zinc within 0.01; the balance, iron. EFFECT: higher efficiency. 3 tbl

Similar patents RU2107107C1

Title Year Author Number
HIGH-TEMPERATURE ALLOY 1994
RU2095458C1
HEAT-RESISTANT ALLOY 2000
RU2194784C2
HEAT-RESISTANT ALLOY 2000
RU2194785C2
HEAT-RESISTANT CHROME-NICKEL ALLOY WITH AUSTENITIC STRUCTURE 2010
  • Afanas'Ev Sergej Vasil'Evich
  • Danil'Chenko Aleksandr Vladimirovich
  • Shevakin Aleksandr Fedorovich
RU2446223C1
REFRACTORY CHROMIUM-NICKEL ALLOY WITH AUSTENITE STRUCTURE 2013
  • Makhlaj Sergej Vladimirovich
  • Afanas'Ev Sergej Vasil'Evich
RU2533072C1
REFRACTORY ALLOY 1998
RU2149210C1
REFRACTORY ALLOY 1998
RU2149208C1
HEAT RESISTANT ALLOY 2009
  • Makhlaj Vladimir Nikolaevich
  • Afanas'Ev Sergej Vasil'Evich
  • Roshchenko Ol'Ga Sergeevna
RU2393260C1
HEAT-RESISTANT ALLOY 2000
RU2194786C2
REFRACTORY ALLOY 1998
RU2149211C1

RU 2 107 107 C1

Authors

Dates

1998-03-20Published

1996-01-03Filed