FIELD: finishing materials for leveling concrete and plaster surfaces. SUBSTANCE: spackling compound comprises, wt %: hydrated lime, 45-50.09; water, 27-33.46; polyacrylamide, 4.2-6.15; aqueous emulsion of 30% polystyrene foam solution in gasoline-acetone solvent mixture at 1:1 ratio, 14-20.1. EFFECT: shorter drying time and greater cohesion strength. 2 tbl