FIELD: application of protective coats. SUBSTANCE: impregnation is effected in emulsion on base of AVTOCAT F-78 containing additionally carbamide in the amount of 2 to 4 g/l; concentration of AVTOCAT F-78 ranges from 50 to 100 g/l at temperature of treatment ranging from 20 to 60 C. EFFECT: enhanced technological and economical efficiency due to reduced concentration of AVTOCAT F-78 and temperature with no change is protective capacity. 1 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITION FOR IMPREGNATION OF PHOSPHATECOATING (TWO VERSIONS) | 2007 |
|
RU2349680C2 |
COMPOSITION AND METHODS OF APPLICATION OF PHOSPHATE AND CHROMIUM COATS | 2001 |
|
RU2209857C1 |
SOLUTION FOR PHOSPHATING | 2005 |
|
RU2283896C1 |
LUBRICATING FLUID CONCENTRATE | 2001 |
|
RU2208046C2 |
METHOD TO APPLY PROTECTIVE POLYMER COATING ONTO SURFACE OF STEEL CARTRIDGE CASE | 2010 |
|
RU2423552C1 |
LUBRICATING FLUID CONCENTRATE FOR MECHANICAL CONVERSION OF METALS | 1998 |
|
RU2135550C1 |
METHOD FOR COOLING TOOL | 2001 |
|
RU2192951C2 |
SORBENT-CATALYST PREPARATION METHOD | 2002 |
|
RU2202410C1 |
SOLUTION FOR PHOSPHATING THE METALLIC SURFACE | 1995 |
|
RU2090650C1 |
METHOD OF PHOSPHATING STEEL PARTS | 2005 |
|
RU2285745C1 |
Authors
Dates
2002-09-27—Published
2000-08-01—Filed