FIELD: oil and gas production. SUBSTANCE: grouting mortar contains, weight parts: cement 100, polysaccharide based on cellulose ether (polycyanine cellulose) 0.1-0.5, ethyl silicate 0.1-1.0, and water 35-50. In another variant of process, mortar also contains 0.2 to 3.9 wt parts of amorphous alumina. EFFECT: lowered filtration within wide temperature range (up to 100 C), increased strength of cement stone, and increased mobility of mortar without increase in water content. 2 cl, 2 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PREPARATION OF GROUTING COMPOSITION | 2001 |
|
RU2186942C1 |
BASE OF DENSIFIED GROUTING MORTAR MAINLY USED IN FRACTURED CARBONATE RESERVOIRS | 2004 |
|
RU2259467C1 |
METHOD OF PREPARATION OF LIGHT-WEIGHT GROUTING MORTAR | 2002 |
|
RU2215124C1 |
EXPANDING PLUGGING MATERIAL | 2007 |
|
RU2360940C1 |
METHOD OF BOTTOM-HOLE REGION LINING | 2010 |
|
RU2467156C2 |
METHOD OF PREPARATION OF LIGHT GROUTING MORTAR OF DENSITY 1450-1500 kg/m | 2008 |
|
RU2385894C1 |
PLUGGING MATERIAL FOR MAKING OF BRIDGES IN WELL DRILLED INVERTED-EMULSION DRILLING MUD (VERSIONS) | 2013 |
|
RU2525408C1 |
BACKFILL FOR CEMENTING WELLS WITH HIGH GAS RATIO | 2011 |
|
RU2447123C1 |
LIGHT-WEIGHT OIL-WELL CEMENT MIX (VARIANTS) | 2003 |
|
RU2256774C2 |
LIGHT-WEIGHT PLUGGING MORTAR | 2000 |
|
RU2196876C2 |
Authors
Dates
2002-10-20—Published
2001-05-23—Filed