FIELD: construction engineering; applicable in construction of main pipelines. SUBSTANCE: steel isolated pipeline is laid into trench on preparation layer treated with binder, filling of cushioning layer of ground treated with binder and filling up of pipeline with ground. Preparation layer contains organic binder in amount of 10-15% of ground weight. Cushioning layer amounts to 8-12% of ground weight. Filling layer and fill ground also contain organic binder in amount of 8-12% of ground weight. EFFECT: increased pipeline reliability. 3 cl, 1 dwg
Title | Year | Author | Number |
---|---|---|---|
METHOD OF LAYING PIPE LINE | 2002 |
|
RU2205316C1 |
METHOD OF LAYING PIPE LINE | 2002 |
|
RU2205315C1 |
METHOD OF REPAIR OF ANTICORROSIVE INSULATION OF SUBTERRANEAN PIPE LINES | 2001 |
|
RU2183783C1 |
METHOD OF REPAIR OF INSULATING COATINGS | 2001 |
|
RU2197668C2 |
PIPELINE ROUTING METHOD | 2014 |
|
RU2559222C1 |
GAS AND OIL PIPELINE LAYING TECHNIQUE | 2014 |
|
RU2559218C1 |
METHOD FOR PROTECTING LOCAL DAMAGED PORTIONS OF INSULATING COATING OF METAL PIPELINES FROM UNDERGROUND CORROSION | 2001 |
|
RU2200774C2 |
METHOD OF REPAIRING BITUMINOUS AND POLYMERIC FILM INSULATOR OF UNDERGROUND PIPE LINE | 0 |
|
SU1687993A1 |
UNDERGROUND PIPELINE LAYING METHOD | 0 |
|
SU932087A1 |
METHOD FOR PROTECTING FROM UNDERGROUND CORROSION IN LOCAL DAMAGED PORTIONS OF ISOLATING COATING OF METAL PIPELINES FREE OF ELECTROCHEMICAL PROTECTION | 2000 |
|
RU2200773C2 |
Authors
Dates
2002-10-20—Published
2001-02-08—Filed