FIELD: ore dressing.
SUBSTANCE: sodium hydroxide solution, prior to me used for saponification of fatty acids, is additionally agitated for 10-15 min with oxide of a metal exhibiting amphoteric properties taken in amount of 0.1% of the weight of fatty acids and with predetermined volume of water until desired sodium salt is obtained. After that, fatty acid is added and saponification reaction is carried out at stirring for 25-30 min. Ratio of sodium hydroxide, amphoteric metal oxide, and fatty acid under stirring at 40-50оС equals 1.005:0.005:5.
EFFECT: enhanced flotation activity of collector resulting in higher recovery of non-sulfide minerals into concentrate.
1 tbl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
FLOTATION OF IRON-BEARING TUNGSTEN MINERALS FROM ORE GRAVITY DRESSING SLIMES | 2014 |
|
RU2569660C2 |
FLOTATION COLLECTOR FOR NON-SULPHIDE ORES | 0 |
|
SU876173A1 |
FLOTATION COLLECTOR FOR NON-SULFIDE ORES AND A METHOD OF ITS PRODUCTION | 2003 |
|
RU2255813C1 |
METHOD OF FLOTATION OF BARITE-CONTAINING ORES | 2000 |
|
RU2182042C2 |
METHOD OF IRON-ORE BENEFICATION | 0 |
|
SU1488012A1 |
PHOSPHATE ORE PROCESSING METHOD | 2017 |
|
RU2722484C1 |
METHOD OF CALCITO-FLUORITE ORES FLOTATION | 2001 |
|
RU2192314C1 |
GATHERER FOR FLOTATION OF APATITE-CONTAINING ORES | 0 |
|
SU1005361A1 |
METHOD OF EXTRACTION OF OXIDIZED MOLYBDENUM AT PROCESSING OF MIXED MOLYBDENUM ORES | 2002 |
|
RU2234548C2 |
METHOD OF FLOTATION OF NON-SULPHIDE ORES | 0 |
|
SU1528567A1 |
Authors
Dates
2004-08-27—Published
2002-05-06—Filed