FIELD: oil and gas extractive industry.
SUBSTANCE: method includes mixing of cementing cement with micro-spheres and mixing with liquid, previously a dry powder-like polymer water output reducer is mixed with micro-spheres with following relation to weight of cementing cement in percents of mass: micro-spheres 10-45, water output reducer - 0.15-0.45, mixture of these admixtures is mixed with said cement and then mixed with liquid - previously prepared 0.02-0.08% solution of foam suppressant tributylphosphate with water-hard relation 0.6-0.85. As dry powder like polymer water output reducers sulphocell, camcell, oxyethylcellulose, polyvinyl spirits, polyacrylamide are used.
EFFECT: low density - up to 1200 kg/m3, low density oscillations during mixing - ±20 kg/m3, lower bed repression, prevented absorption of cementing solution, assured rise of cement to projected height.
1 ex, 2 cl
Title | Year | Author | Number |
---|---|---|---|
RAW MIXTURE FOR OBTAINING LIGHT-WEIGHT GROUTING MORTAR | 2011 |
|
RU2472835C1 |
METHOD OF PREPARATION OF LIGHT-WEIGHT GROUTING MORTAR | 2002 |
|
RU2215124C1 |
METHOD OF PREPARATION OF LIGHT GROUTING MORTAR OF DENSITY 1450-1500 kg/m | 2008 |
|
RU2385894C1 |
METHOD FOR REPAIR AND INSULATION WORK IN THE WELL | 2022 |
|
RU2783449C1 |
METHOD FOR REPAIR AND INSULATION WORK IN WELL (OPTIONS) | 2020 |
|
RU2750414C1 |
LIGHT-WEIGHT GASPROOF PLUGGING MATERIAL FOR CEMENTING OVER-PRODUCING INTERVALS (VERSIONS) | 2012 |
|
RU2497861C1 |
EXPANDING PLUGGING MATERIAL | 2007 |
|
RU2360940C1 |
CEMENT GROUTING LIGHT-WEIGHT MIXTURE | 2009 |
|
RU2399643C1 |
LIGHTWEIGHT PLUGGING COMPOSITION | 2014 |
|
RU2588026C1 |
METHOD OF PREPARING LIGHT-WEIGHT GROUTING MORTAR | 2000 |
|
RU2172812C2 |
Authors
Dates
2004-10-27—Published
2003-08-18—Filed