FIELD: oil and gas extractive industry.
SUBSTANCE: mixture contains, in percents of mass: Portland cement 85-89.5, expanded vermiculite sand 2-5, alumosilicate microspheres 2-5, granulated calcium chloride, as stabilizing admixture, - the rest.
EFFECT: higher stability and efficiency.
1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| LIGHT-WEIGHT PLUGGING MIX | 2004 |
|
RU2255205C1 |
| LIGHT-WEIGHT GROUTING MIX | 2000 |
|
RU2187621C1 |
| LIGHTWEIGHT PLUGGING MATERIAL | 2013 |
|
RU2555165C2 |
| LIGHT-WEIGHT PLUGGING MIXTURE | 1998 |
|
RU2139409C1 |
| OIL-WELL LIGHT WEIGHT PORTLANDCEMENT | 2013 |
|
RU2523588C1 |
| PLUGGING MIX | 2003 |
|
RU2245989C1 |
| SALT-SATURATED PLUGGING COMPOSITION FOR HIGH-TEMPERATURE HOLES | 2004 |
|
RU2273654C1 |
| LIGHT-WEIGHT GASPROOF PLUGGING MATERIAL FOR CEMENTING OVER-PRODUCING INTERVALS (VERSIONS) | 2012 |
|
RU2497861C1 |
| METHOD OF PREPARATION OF LIGHT GROUTING MORTAR OF DENSITY 1450-1500 kg/m | 2008 |
|
RU2385894C1 |
| METHOD OF PREPARATION OF LIGHT-WEIGHT GROUTING MORTAR | 2002 |
|
RU2215124C1 |
Authors
Dates
2004-12-27—Published
2003-04-29—Filed