FIELD: rolled tube production, namely method for making pilger mill mandrels from heat resistant steel for rolling hot rolled tubes.
SUBSTANCE: method for making mandrels used for rolling hot rolled tubes with large and mean diameters in range 273-550mm comprises steps of casting ingots of hear resistant steel; forging cylindrical solid or hollow blanks, roughly working of them, performing heat treatment and finishing mandrels at forming conicity 1 - 2 mm on length of their working portion while taking into account designed linear expansion coefficient during rolling process; determining diameter size by means of expression δ = dn - Δ/1 + α·t. One portion of mandrel from lock along length of half of working portion of mandrel is in the form of cone with diameters of cone bases determined form given expression and second portion is in the form of cylinder or truncated cone whose diameters are determined according to next expression
EFFECT: lowered lengthwise thickness difference of tubes.
3 cl, 1 dwg, 1 tbl
Title | Year | Author | Number |
---|---|---|---|
COMPOSITE MANDREL FOR LARGE- AND MEDIUM-DIAMETER PIPE PILGER ROLLING | 2012 |
|
RU2527589C2 |
PRODUCTION AND OPERATION OF PILGER MILL COMPOSITE MANDRELS FOR PRODUCTION OF LARGE- AND MEDIUM-DIAMETER HOT-ROLLED PIPES | 2012 |
|
RU2523395C2 |
METHOD FOR MAKING TUBES OF HARD-TO-FORM STEELS AND ALLOYS WITH INCREASED COEFFICIENT OF LINEAR EXPANSION | 2001 |
|
RU2214312C2 |
PRODUCTION AND OPERATION OF PILGER MILL COMPOSITE MANDRELS FOR PRODUCTION OF LARGE- AND MEDIUM-DIAMETER HOT-ROLLED PIPES | 2012 |
|
RU2523179C2 |
METHOD FOR MAKING AND EXPLOITING DRIFTS OF PILGER MILLS FOR PRODUCING HOT ROLLED TUBES OF LARGE AND MEAN DIAMETERS | 2006 |
|
RU2322318C2 |
METHOD FOR MAKING PILGER MILL MANDREL AND EXPLOITING IT | 2003 |
|
RU2248853C2 |
METHOD OF PRODUCTION AND OPERATION OF PILGER MILL MANDRELS | 2006 |
|
RU2328354C2 |
METHOD OF PRODUCTION OF TRIBLETS OF PILGRIM-STEP ROLLING MILLS | 2003 |
|
RU2256708C2 |
METHOD FOR MAKING MANDRELS OF PILGER ROLLING MILLS | 2003 |
|
RU2249052C2 |
RECONDITIONING OF PILGER MILL MANDREL USED FOR HOT ROLLED 273-550 mm-DIA PIPES MADE OF "25-2¦1L"-GRADE STEEL WITH INITIAL SURFACE SORBITE PLY DEPTH OF 40-50 mm | 2013 |
|
RU2537340C2 |
Authors
Dates
2005-01-10—Published
2003-02-06—Filed