FIELD: pretreatment of fine crushed fluorspar concentrates useful as flux in metallurgy.
SUBSTANCE: claimed method includes agitation of concentrate with 8-18 % humidity, calcium hydroxide or calcium oxide and treacle in wt % of 1-2 and 2-6 as reduced to concentrate mass, respectively. Obtained wet mass if extruded through nozzle, cut to the desired dimensions, dried for 10-30 min at 60-1200C, and held at positive temperature for at least 5 days.
EFFECT: method for agglomeration of fine crushed fluorspar concentrates with increased humidity to obtain product of desired strength.
1 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF BRIQUETTING FLOATATION FLUORITE CONCENTRATES | 2004 |
|
RU2268314C1 |
AGGLOMERATION METHOD OF CRUSHED PRODUCTS | 2012 |
|
RU2490339C1 |
METHOD OF EXTRACTION OF NOBLE METALS FROM GRAVITATIONAL SILICATE CONCENTRATES CONTAINING GOLD AND SILVER | 2002 |
|
RU2221062C1 |
METHOD FOR EXTRACTION OF GERMANIUM | 2008 |
|
RU2375481C1 |
METHOD FOR PRODUCING EXTRUSION-TYPE BRIQUETTE (BREKS) FOR METAL MELTING | 2012 |
|
RU2506325C2 |
CHARGE FOR PRODUCING UNCALCINED NODULIZED INITIAL ORE MATERIAL | 0 |
|
SU1474176A1 |
METHOD OF LUMPING WITHOUT FIRING | 0 |
|
SU989874A1 |
IRON-CONTAINING MATERIAL PROCESSING METHOD | 2011 |
|
RU2466196C1 |
METHOD OF LUMPING DISPERSE MATERIALS | 0 |
|
SU1520123A1 |
METHOD OF PRODUCING MANGANESE CONTAINING BRIQUETTES | 0 |
|
SU1698305A1 |
Authors
Dates
2005-02-10—Published
2003-03-21—Filed