FIELD: polymer materials.
SUBSTANCE: sound-insulation film for manufacturing layered shatterproof glasses contains 0.15-0.8 % water; 50-79.85% partially acetylated polyvinyl alcohol having 10-25% vinyl alcohol groups and 0-20% acetate groups; and 20-49.85% plasticizer. The latter contains 30 to 70 % by weight of (based on the total weight of plasticizer mixture) one or several poly(alkylene glycols) from group including poly(alkylene glycols) having general formula HO-(R-O)nH wherein R represents ethylene, propylene, or butylene and n>5; block copolymers from ethylene and propylene glycols having general formula HO-(CH2-CH2-O)n-(CH2-CH(CH3)-O)mH wherein n>2, m>3, and (n+m)<25; derivatives of block copolymers from ethylene and propylene glycols having general formulas R1O-(CH2-CH2-O)n-(CH2-CH(CH3)-O)mH and HO-(CH2-CH2-O)n-(CH2-CH(CH3)-O)m-R1 wherein n>2, m>3, and (n+m)<25 and R1 is organic residue with 1 to 15 carbon atoms; poly(alkylene glycol) derivatives having general formula R1-O-(R2-O)nH wherein R2 represents ethylene, propylene, or butylene and n ≥ 2, in which hydrogen atom of two terminal hydroxyl groups of poly(alkylene glycol) is substituted by organic residue R1; and at least one plasticizer - the rest.
EFFECT: improved sound-insulation capacity of film even at ambient temperature.
1 dwg, 2 tbl, 11 ex
Authors
Dates
2006-02-20—Published
2000-08-16—Filed