FIELD: facing materials.
SUBSTANCE: invention relates to fritted glaze compositions. Proposed glaze comprises the following components, wt.-%: SiO2, 58.0-60.0; Al2O3, 4.0-6.0; CaO, 8.0-10.0; K2O, 4.0-5.0; B2O3, 6.0-8.0; MgO, 1.0-3.0; CuO, 1.0-2.0, and TiO2, 10.0-14.0. Invention provides enhancing thermal stability of glaze. Proposed compositions can be used for coating facing tile and articles of economy-domestic designation.
EFFECT: improved and valuable property of glaze.