FIELD: coating and facing materials.
SUBSTANCE: invention proposes glaze comprising the following components, wt.-%: SiO2, 50.0-56.0; Al2O3, 4.0-5.0; CaO, 4.0-5.0; MgO, 1.0-2.0; K2O, 3.0-4.0; B2O3, 10.0-12.0; SnO2, 4.0-5.0; SrO, 4.0-5.0; TiO2, 6.0-10.0, and ZrO2, 4.0-6.0. Invention provides enhancing thermal stability of glaze. The proposed glaze is used for applying on articles made of porcelain and other ceramics.
EFFECT: improved property of glaze.