FIELD: chemistry.
SUBSTANCE: invention pertains to glazing compounds and can be used in making faced tiles. The glaze consists of the following components with the given percentage mass ratios: SiO2 45.0-47.0; Al2O3 8.0-10.0; MgO 1.0-2.0; Na2O 1.0-2.0; CaO 6.0-8.0; Fe2O3 0.3-0.7; CuO 0.7-1.3; K2O 1.0-2.0; BaO 3.0-4.0; PbO 15.0-18.0; TiO2 4.0-6.0; B2O3 6.0-8.0.
EFFECT: increased frost resistance of the glaze.
1 tbl