FIELD: chemistry.
SUBSTANCE: ceramic mixture consists of the following percentage mass ratios: 40-42% raw clay; 10-15% wollastonite; 15-20% pyrophillite; 10-15% quartz; 2-3% mica; 2-3% calcite; 2-3% perovskite; 8-10% nepheline. The bending strength of the tile is 35-40 MPa.
EFFECT: increased strength of the product made from the mixture.
1 tbl