FIELD: chemistry.
SUBSTANCE: invention concerns galvanic technique. The electrolyte contains, in g/l: nickel sulfate 15-22; cobalt sulfate 18-22; trilon B 28-32; 1,4-butanediol, in ml/l 0.8-1.2; boric acid 28-32; sodium sulfate 114-170, and water.
EFFECT: improved gleam and corrosion resistance of coatings.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
ELECTROLYTE FOR PRECIPITATING CADMIUM-NICKEL ALLOY | 2006 |
|
RU2333295C2 |
ELECTROLYTE FOR SEDIMENTATION OF COATINGS OUT OF CADMIUM-IRON ALLOY | 2006 |
|
RU2334832C1 |
ELECTROLYTE FOR SEDIMENTATION OF COATINGS OUT OF CADMIUM-COBALT ALLOY | 2006 |
|
RU2334833C1 |
CADMIUM-ZINC PLATING DEPOSITION ELECTROLYTE | 2007 |
|
RU2350697C1 |
ELECTROLYTE FOR COATING SEDIMENTATION MADE OF ALLOY LEAD-ZINC | 2007 |
|
RU2353715C1 |
ELECTROLYTE FOR COATING DEPOSITION FROM CADMIUM AND MANGANESE MELT | 2007 |
|
RU2350696C1 |
ELECTROLYTE FOR PRECIPITATING CADMIUM-CHROME ALLOY COATINGS | 2006 |
|
RU2333296C1 |
ELECTROLYTE FOR DEPOSITION OF COATINGS FROM ZINC-COBALT ALLOY | 2023 |
|
RU2820290C1 |
ELECTROLYTE FOR DIRECT NICKEL-PLATING OF ALUMINIUM AND ITS ALLOYS | 1992 |
|
RU2061104C1 |
AQUEOUS ELECTROLYTE FOR BRIGHT NICKEL-PLATING, ITS VARIANT | 1993 |
|
RU2071996C1 |
Authors
Dates
2008-09-10—Published
2006-11-21—Filed