FIELD: metallurgy.
SUBSTANCE: method includes dry breaking and grinding of ore to size of not more, than 1.0-4.0 mm, ore leaching and mixing, when contents of solid phase is 50-70% with solution of sulphuric acid of 10.0 to 40 g/dcm3 within 0.5-2.0 hrs. After leaching generated cake is dehydrated, washed, subject to neutralisation and crushed to size of 60-95% class - 0.074 mm. Flotation of copper minerals with production of flotation concentrate is carried out. Solution after leaching of ore and cake wash water are merged and freed from solid suspension; then cathode copper is extracted out of them.
EFFECT: reduced consumption of sulphuric acid and water for process; increased extraction of copper out of ore and upgraded quality of consumer products.
8 cl, 2 ex
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCTION OF CATHODE COPPER OUT OF SULPIDE OXIDISED COPPER ORES | 2007 |
|
RU2336345C1 |
METHOD OF PRODUCTION OF CATHODE COPPER OUT OF SULPHIDE OXIDISED COPPER ORES | 2007 |
|
RU2336344C1 |
METHOD OF PROCESSING OF SULPHIDE OXIDISED COPPER ORES | 2007 |
|
RU2337160C1 |
PROCEDURE FOR PROCESSING MIXED COPPER ORE | 2009 |
|
RU2418872C2 |
PROCEDURE FOR EXTACTION OF METALS FROM GOLD CONTAINING SULPHIDE-OXIDISED COPPER ORES | 2009 |
|
RU2428493C1 |
PROCESSING METHOD OF SULPHIDE-OXIDATED COPPER ORES WITH COPPER AND SILVER EXTRACTION | 2009 |
|
RU2439177C2 |
METHOD FOR COMPLEX PROCESSING OF SULPHIDE-OXIDISED COPPER-PORPHYRITIC ORES | 2018 |
|
RU2685621C1 |
METHOD FOR PROCESSING COPPER CONTAINING PRODUCTS | 2000 |
|
RU2178342C1 |
METHOD FOR PROCESSING MIXED COPPER ORES CONTAINING PRECIOUS METALS | 2009 |
|
RU2404269C1 |
METHOD OF PROCESSING SULPHIDE OXIDISED COPPER ORES WITH COPPER AND SILVER EXTRACTION | 2015 |
|
RU2604279C1 |
Authors
Dates
2008-10-27—Published
2007-04-16—Filed