FIELD: construction.
SUBSTANCE: refractory mixture contains refractory clay, kaolin, heteropolymer of salicylic acid with formaldehyde, lignosulphonates, sodium polyphosphate, chamotte and asbestine, given the following components ratio, wt%: refractory clay - 20.-25.0; kaolin -10.0-15.0; heteropolymer of salicylic acid with formaldehyde, - 0.1-0.2; lignosulphonates - 0.3-0.5; sodium polyphosphate- 0.1-0.2; asbestine - 10.0-15.0; chamotte - the rest.
EFFECT: enhancing strength of the goods.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
CERAMIC MASS | 2007 |
|
RU2345038C2 |
PORCELAIN MASS | 2006 |
|
RU2333899C1 |
PORCELAIN MIXTURE | 2006 |
|
RU2331607C2 |
CERAMIC MIXTURE | 2009 |
|
RU2412924C1 |
CERAMIC BODY FOR MANUFACTURING OF FACING TILES | 2007 |
|
RU2343132C2 |
CERAMIC MIXTURE FOR PRODUCTION OF FLOOR TILES | 2008 |
|
RU2366635C1 |
CERAMIC MIXTURE FOR MAKING TILES | 2010 |
|
RU2413692C1 |
CERAMIC MIXTURE | 2009 |
|
RU2405753C1 |
CHARGE FOR PREPARATION OF LIGHTWEIGHT FIRE RESISTANT MATERIAL | 2007 |
|
RU2351569C2 |
CERAMIC MASS FOR FLOOR TILE PRODUCTION | 2007 |
|
RU2345039C2 |
Authors
Dates
2009-03-10—Published
2007-01-25—Filed