FIELD: metallurgy.
SUBSTANCE: invention relates to metallurgy and can be used in jewellery industry, and also during manufacturing of fine mechanics details. For hardening of alloy it allows following composition, wt %: copper 5.0 - 10.0; nickel 30.0 - 35.0; silver 4.0 - 9.0; gold 50.0 - 55.0; rhenium 0.5 - 1.0. Alloy hardness is 215 - 220 HV.
EFFECT: hardening of alloy.
1 tbl