FIELD: mining engineering.
SUBSTANCE: invention relates to metallurgy and can be used for manufacturing of jewels, coins, flatware. Invention contains, wt %: copper 18.0-20.0; nickel 2.0-2.5; indium 0.5-1.0; tin 0.01-0.02, niobium 0.08-0.12; beryllium 0.01-0.02; silver 76.5-80.0. Tensile strength of alloy is preliminary 70 kilogram-force/mm2.
EFFECT: alloy hardening.