FIELD: mining.
SUBSTANCE: invention is related to mining industry, namely to hardening fill mixtures. It includes filler, liquid sodium glass, gypsum, cement. Fill mixture is additionally supplemented with flocculant and martite-hematite iron ore, with the following ratio of mixture components: liquid sodium glass 20-22%; cement 1-2%; gypsum 1-2%; flocculant 0.002-0.004%; martite-hematite iron ore 1%; filler - the rest.
EFFECT: improved quality of technological properties of hardening fill mixture, reduced prime cost, increased bearing capacity of filled mass, reduced consumption of hardening solution and simplified technology of stripped area filling.
2 cl, 1 tbl
| Title | Year | Author | Number | 
|---|---|---|---|
| HARDENING FILLING MIXTURE | 2020 | 
									
  | 
                RU2747753C1 | 
| SOLIDIFYING CLINKER-FREE STOWING MIX | 2004 | 
									
  | 
                RU2275505C1 | 
| STOWING MIXTURE COMPOSITION | 2018 | 
									
  | 
                RU2721566C1 | 
| METHOD FOR FILLING MASS FORMING OF HARDENING SLAG MIX | 2004 | 
									
  | 
                RU2278273C1 | 
| FILLING MIXTURE COMPOUND | 2011 | 
									
  | 
                RU2462598C1 | 
| MIXTURE FOR FILLING OF WORKED-OUT SPACE | 1995 | 
									
  | 
                RU2100615C1 | 
| METHOD OF PREPARING GOBBING MIXTURE | 1995 | 
									
  | 
                RU2103517C1 | 
| CONSTRUCTION MIXTURE FOR MAKING ROOFING SHEET AND METHOD OF MAKING ROOFING SHEET | 2011 | 
									
  | 
                RU2494990C2 | 
| MIXTURE OF MAKING LIGHT CONCRETE AND LIGHT CONCRETE | 2008 | 
									
  | 
                RU2399598C2 | 
| METHOD OF FLOTATION OF HEMATITE-BEARING IRON ORES AND PRODUCTS | 2012 | 
									
  | 
                RU2494818C1 | 
Authors
Dates
2009-12-27—Published
2008-10-21—Filed