FIELD: physics.
SUBSTANCE: described is a compound consisting of epoxy-diane resin "ЭД-20", amine hardener of ethylenediaminomethylphenol "АФ-2", "ТМФТ" product of a titanium organosilicon oligomer of formula Ti{[OSi(CH3)(C6H5)]2-5OH}4, oligoesterepoxide Laproxide 301, oligoesterepoxide Laproxide 703 and low-molecular polyamide resin "ПО-300". The method of preparing the compound is based on mixing components and their hardening at temperature 25°±10°C for not less than 8 hours, and then at temperature 70-80°C for 2-4 hours.
EFFECT: longer life, wider range of operating temperature and reduced mean square deviation of phase-time characteristics.
2 cl, 2 tbl, 3 ex
Title | Year | Author | Number |
---|---|---|---|
FOAM COMPOUND COMPOSITION | 2009 |
|
RU2428449C2 |
FOAMED COMPOUND COMPOSITION | 2006 |
|
RU2294951C1 |
FOAM COMPOUND COMPOSITION | 2009 |
|
RU2428450C1 |
FOAM COMPOUND COMPOSITION | 2012 |
|
RU2496817C1 |
METHOD OF OBTAINING FOAM COMPOUND | 2007 |
|
RU2326148C1 |
POLYMER COMPOSITION FOR HIGH-FREQUENCY ENERGY ABSORPTION | 2007 |
|
RU2343173C1 |
FOAM COMPOUND COMPOSITION | 2009 |
|
RU2395554C1 |
FOAM COMPOUND COMPOSITION | 2010 |
|
RU2430133C1 |
METHOD OF PRODUCING FOAM COMPOUND | 2009 |
|
RU2408645C2 |
COLD SETTING COMPOUND | 2012 |
|
RU2481373C1 |
Authors
Dates
2010-01-10—Published
2008-02-13—Filed