FIELD: construction engineering.
SUBSTANCE: raw mix for manufacturing of facing tile contains, vol %: asbestos waste 69.0-73.0; Portland cement 15.0-17.0, granules of polystyrene foam of fraction to 10 mm 12.0-14.0 with the water-cement ratio making 0.8-0.85.
EFFECT: reduced water absorption of the tile.
1 cl, 1 tbl