FIELD: construction.
SUBSTANCE: in method for production of gypsum construction material, including treatment phosphogypsum PG or phosphor-semihydrate PSH of calcium sulfate in runner mills after primary filtration PF with introduction of additive for neutralisation of acids, specified treatment is carried out for 4-12 minutes at the pressure of 1.0-6.5 MPa. Afterwards secondary filtration is carried out to reduce moisture of PG or specified PSH twice compared to moisture after PF. It is preferable to do treatment in runners for 8 minutes at the pressure of 1.0 MPa.
EFFECT: quicker hardening.
2 cl, 3 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
METHOD OF PRODUCING WATER-RESISTANT GYPSUM BUILDING MATERIALS | 2008 |
|
RU2413689C2 |
METHOD OF PREPARING CALCIUM PHOSPHOSEMIHYDRATE FOR USE IN CEMENT PRODUCTION | 0 |
|
SU1530595A1 |
BUILDING MATERIAL PRODUCING METHOD | 0 |
|
SU1775385A1 |
METHOD OF MAKING BINDER | 2008 |
|
RU2389701C1 |
METHOD OF PRODUCING BINDING MATERIALS MAINLY CONSISTING OF CALCIUM AND MAGNESIUM OXIDES | 2010 |
|
RU2479509C2 |
METHOD OF CALCIUM SULPHATE PHOSPHOSEMIHYDRATE PROCESSING | 2009 |
|
RU2396209C1 |
METHOD OF PRODUCING FOAMED POROUS AGGREGATES | 2012 |
|
RU2526034C2 |
METHOD OF PREPARING RAW MIXTURE FOR BUILDING ARTICES | 0 |
|
SU1235843A1 |
METHOD FOR PRODUCTION GYPSUM BIDING AGENT OF PHOSPHOGYPSUM | 0 |
|
SU1794925A1 |
METHOD OF PRODUCING ANHYDRIDE BINDER FROM PHOSPHOGYPSUM | 0 |
|
SU1694533A1 |
Authors
Dates
2010-09-27—Published
2008-12-31—Filed