FIELD: construction.
SUBSTANCE: raw mix for production of an artificial porous filler contains the following components, wt %: low melting clay 25.0 - 35.0, dried slag of crystal cutting 65.0 - 75.0.
EFFECT: reduced baking temperature.
1 tbl