FIELD: construction.
SUBSTANCE: ceramic mass contains clay, phosphorous slag and marshallite, at the following ratio of components, wt %: clay - 78-86; phosphorous slag - 4-8; marshallite - 10-14.
EFFECT: improved thermal resistance of products.