FIELD: metallurgy.
SUBSTANCE: invention refers to compositions of copper-based alloys which can be used for manufacture of housings of watches and coins. Copper-based alloy contains the following, wt %: beryllium 0.01-0.02; silver 6.0-8.0; zinc 26.0-32.0; gold 0.01-0.02; copper is the rest.
EFFECT: increasing alloy fluidity.
1 tbl