FIELD: oil-and-gas production.
SUBSTANCE: proposed acid-soluble backfill composition comprises backfill Portland cement, dust from electric filters of cement plants, admixture of silica-alumina composition and water. Additionally, it includes gypsum-alumina expanding cement and super plasticiser "ЦЕМПЛАСТ МФ" or Melflux and silica-alumina microspheres as said admixture at the following ratio of components, in wt % backfill Portland cement 17.6-33.5, gypsum-alumina expanding cement 3.3-17.6, said cement dust 3.3-20.1, said super plasticiser 0.06-0.13, silica-alumina microspheres 6.7-30.0, water 32.8-41.3.
EFFECT: complete acid-solubility of cement stone, higher strength.
1 ex, 2 tbl
Title | Year | Author | Number |
---|---|---|---|
ACID-SOLUBLE LIGHTWEIGHT PLUGGING MATERIAL TO LIQUIDATE ABSORPTION IN PRODUCTIVE FORMATIONS | 2014 |
|
RU2575489C1 |
EXPANDING PLUGGING MATERIAL | 2007 |
|
RU2360940C1 |
GROUTING MORTAR FOR CEMENTING HORIZONTAL HOLES | 2012 |
|
RU2508307C2 |
OIL-WELL COMPOSITION FOR STEAM-INJECTION WELLS | 2007 |
|
RU2359988C1 |
FIBRE-REINFORCED PLUGGING MATERIAL FOR CEMENTING PRODUCTION INTERVALS SUBJECT TO PERFORATION DURING WELL DEVELOPMENT | 2011 |
|
RU2458962C1 |
LIGHT-WEIGHT GASPROOF PLUGGING MATERIAL FOR CEMENTING OVER-PRODUCING INTERVALS (VERSIONS) | 2012 |
|
RU2497861C1 |
GROUTING MORTAR BASE FOUNDATION FOR WELL CEMENTING | 2007 |
|
RU2337124C1 |
METHOD OF PREPARATION OF LIGHT GROUTING MORTAR OF DENSITY 1450-1500 kg/m | 2008 |
|
RU2385894C1 |
PLUGGING MATERIAL FOR MAKING OF BRIDGES IN WELL DRILLED INVERTED-EMULSION DRILLING MUD (VERSIONS) | 2013 |
|
RU2525408C1 |
BACKFILL FOR CEMENTING WELLS WITH HIGH GAS RATIO | 2011 |
|
RU2447123C1 |
Authors
Dates
2012-06-10—Published
2010-12-06—Filed