FIELD: chemistry.
SUBSTANCE: crude mixture for making porous aggregate contains the following in wt %: montmorillonite clay 40.0-60.0; kyanite ground to specific surface area 4000-4500 cm2/g 20.0-30.0; silicate glass ground to specific surface area 4000-4500 cm2/g 20.0-30.0.
EFFECT: high strength.
1 tbl
| Title | Year | Author | Number |
|---|---|---|---|
| RAW MIX FOR MANUFACTURING OF POROUS FILLER | 2011 |
|
RU2443656C1 |
| MIXURE FOR MAKING POROUS AGGREGATE | 2009 |
|
RU2411202C1 |
| RAW MIX FOR MAKING HEAT INSULATION ITEMS | 2011 |
|
RU2469989C1 |
| CRUDE MIXTURE FOR MAKING HEAT-INSULATION ARTICLES | 2012 |
|
RU2495843C1 |
| CRUDE MIXTURE FOR MAKING POROUS AGGREGATE | 2012 |
|
RU2489377C1 |
| CHARGE FOR PRODUCTION OF POROUS FILLER | 2013 |
|
RU2528312C1 |
| MIXTURE FOR MAKING POROUS AGGREGATE | 2011 |
|
RU2455247C1 |
| MIXTURE FOR MAKING POROUS AGGREGATE | 2011 |
|
RU2466113C1 |
| MIXURE FOR MAKING POROUS AGGREGATE | 2009 |
|
RU2411203C1 |
| CRUDE MIXTURE FOR MAKING POROUS AGGREGATE | 2012 |
|
RU2489376C1 |
Authors
Dates
2012-09-27—Published
2011-10-24—Filed