FIELD: chemistry.
SUBSTANCE: invention relates to silicate coating compositions for applying on ceramic bricks. The silicate coating contains the following components, pts.wt: ground feldspar 28-30; ground quartz 10-12; ground lime 4-6; ground scrap porcelain 4-6; ground scrap sheet glass 48-52.
EFFECT: low firing temperature of the silicate coating.