FIELD: chemistry.
SUBSTANCE: adhesive composition contains polychloroprene rubber nairit, butyl phenol-formaldehyde resin, thiuram, zinc oxide, magnesium oxide, an organic solvent and a modifier. The organic solvent is a mixture of ethyl acetate and nefras. The modifier used is modified carbon fibre with size of 2-3 mm. The modified carbon fibre is obtained by pyrolysis at 400°C for 30 minutes of polyvinyl alcohol fibre, treatment with methylphosphite borate, followed by treatment of the obtained carbon fibre with a mixture of methylphosphite borate and triethanolamine at 80°C.
EFFECT: invention increases strength of glued vulcanised rubber.
2 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
ADHESIVE COMPOSITION | 2011 |
|
RU2470975C1 |
ADHESIVE COMPOSITION | 2011 |
|
RU2470974C1 |
METHOD OF GLUING RUBBER | 2011 |
|
RU2470973C1 |
ADHESIVE COMPOSITION | 2011 |
|
RU2470976C1 |
ADHESIVE COMPOSITION | 2009 |
|
RU2393192C1 |
ADHESIVE COMPOSITION | 2011 |
|
RU2487153C1 |
ADHESIVE COMPOSITION | 2011 |
|
RU2479612C1 |
ADHESIVE COMPOSITION | 2009 |
|
RU2393194C1 |
COMPOSITION FOR FIRE-RETARDANT RUBBER COATINGS | 2015 |
|
RU2616068C1 |
ADHESIVE COMPOSITION | 2009 |
|
RU2434031C2 |
Authors
Dates
2013-04-20—Published
2011-10-25—Filed