FIELD: chemistry.
SUBSTANCE: invention relates to foundry. The suspension contains the following components in wt %: water 14-18, clay 1-2, electrolyte 0.05-0.2, powdered graphite 3-6, refractory filler - the balance. The refractory filler used is a mixture of quartz sand which is taken in amount of 60-70 wt % and marshalite.
EFFECT: improved heat resistance of shell moulds and high quality of moulding.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
SUSPENSION FOR MAKING PRECISION CASTING MOULDS BY ELECTROPHORESIS | 2011 |
|
RU2481917C1 |
SUSPENSION FOR MAKING PRECISION CASTING MOULDS BY ELECTROPHORESIS | 2010 |
|
RU2443501C1 |
SUSPENSION FOR MAKING PRECISION CASTING MOULDS BY ELECTROPHORESIS | 2010 |
|
RU2443500C1 |
SUSPENSION BY MAKING CERAMIC MOULDING TOOL BY ELECTROPHORESIS | 2011 |
|
RU2470734C1 |
SUSPENSION FOR MAKING CERAMIC MOLDS BY ELECTROPHORESIS PROCESS | 2005 |
|
RU2316406C2 |
SUSPENSION FOR MAKING PRECISION CASTING MOULDS BY ELECTROPHORESIS | 2011 |
|
RU2481172C2 |
SUSPENSION FOR MAKING PRECISE CASTING MOLDS BY ELECTROPHORESIS METHOD | 2006 |
|
RU2298448C1 |
METHOD OF MAKING INVESTMENT PATTERNS FOR PRODUCTION OF SHELL MOULDS BY ELECTROPHORESIS | 2011 |
|
RU2488459C1 |
SUSPENSION FOR ELECTROFORETICALLY PRODUCING CASTING MOLDS USING TEMPORARY PATTERNS | 0 |
|
SU722649A1 |
SUSPENSION FOR OBTAINING CERAMIC MOULDS BY ELECTROPHORESIS METHOD | 0 |
|
SU621439A1 |
Authors
Dates
2013-07-27—Published
2011-10-21—Filed