FIELD: chemistry.
SUBSTANCE: charge for obtaining decorative-facing material includes milled glass, milled natural volcanic slag, kaolin and borax with the following component ratio, wt %: milled glass - 56.0-69.0; milled natural volcanic slag - 25.0-35.0; kaolin - 3.0-7.0; borax - 2.0-3.0.
EFFECT: increased frost resistance of products.
1 tbl
Title | Year | Author | Number |
---|---|---|---|
DECORATIVE FACING MATERIAL | 2010 |
|
RU2417163C1 |
CHARGE FOR OBTAINING DECORATIVE-FACING MATERIAL | 2013 |
|
RU2526070C1 |
MIXTURE FOR PRODUCING DECORATIVE FACING MATERIAL | 2012 |
|
RU2479508C1 |
DECORATIVE FACING MATERIAL | 2006 |
|
RU2332377C2 |
MIXTURE FOR PRODUCING DECORATIVE-CLADDING MATERIAL | 2011 |
|
RU2481308C1 |
DECORATIVE FACING MATERIAL | 2010 |
|
RU2430047C1 |
CERAMIC MUXTURE FOR FACING TILE MANUFACTURE | 2014 |
|
RU2548454C1 |
RAW MATERIAL MIXTURE FOR IMITATION OF NATURAL STONE | 2011 |
|
RU2473496C1 |
CHARGE FOR PRODUCING DECORATIVE-FACING MATERIAL | 2017 |
|
RU2665081C1 |
CRUDE MIXTURE FOR MAKING MATERIAL IMITATING NATURAL STONE | 2013 |
|
RU2508267C1 |
Authors
Dates
2014-01-27—Published
2012-10-05—Filed