CERAMIC MIXTURE FOR MAKING FACING TILE Russian patent published in 2014 - IPC C04B33/04 

Abstract RU 2513669 C1

FIELD: chemistry.

SUBSTANCE: ceramic mixture for making facing tiles contains the following, wt %: kaolin 3.0-4.0; clay 70.0-71.3; potsherd 10.0-15.0; flue ash 10.0-15.0; liquid potassium glass 0.7-1.1. The tiles are fired at 960-970°C.

EFFECT: low firing temperature of the facing tiles.

1 tbl

Similar patents RU2513669C1

Title Year Author Number
CERAMIC MASS FOR MAKING OF FACING TILES 2013
  • Shchepochkina Julija Alekseevna
RU2516175C1
CERAMIC MIXTURE FOR MAKING FACING TILES 2010
  • Shchepochkina Julija Alekseevna
RU2439028C1
CERAMIC MIXTURE 2013
  • Shchepochkina Julija Alekseevna
RU2536597C1
CERAMIC MIXTURE FOR MAKING FACING TILE 2012
  • Shchepochkina Julija Alekseevna
RU2498956C1
CERAMIC MIXTURE FOR MAKING FACING TILES 2011
  • Shchepochkina Julija Alekseevna
RU2449969C1
CERAMIC PASTE FOR PRODUCTION OF FACING TILES 2012
  • Shchepochkina Julija Alekseevna
RU2505509C1
CERAMIC MIXTURE 2011
  • Shchepochkina Julija Alekseevna
RU2458020C1
CERAMIC MIXTURE FOR MAKING FACING TILES 2011
  • Shchepochkina Julija Alekseevna
RU2449968C1
CERAMIC PASTE FOR MANUFACTURE OF FACED TILES 2014
  • Shchepochkina Julija Alekseevna
RU2546181C1
CERAMIC MIXTURE FOR FACING TILE FABRICATION 2011
  • Shchepochkina Julija Alekseevna
RU2469982C1

RU 2 513 669 C1

Authors

Shchepochkina Julija Alekseevna

Dates

2014-04-20Published

2013-03-13Filed