FIELD: metallurgy.
SUBSTANCE: proposed method comprises holding in austenite region at 1060°C for 30-40 min with subsequent air cooling two-step tempering. At first step, low-temperature tempering is performed at 200-350°C while at second step it is performed at 760°C. Every tempering takes 3 hours.
EFFECT: higher long-term strength and creep limit.
4 tbl, 1 ex
Title | Year | Author | Number |
---|---|---|---|
TREATMENT METHOD OF HEAT-RESISTANT MARTENSITE STEEL | 2018 |
|
RU2696302C1 |
METHOD FOR PROCESSING HEAT-RESISTANT LOW-CARBON MARTENSITIC STEELS | 2022 |
|
RU2789958C1 |
METHOD OF THERMOMECHANICAL TREATMENT OF HEAT-RESISTANT STEEL OF MARTENSITIC CLASS | 2018 |
|
RU2688017C1 |
HEAT-RESISTANT STEEL OF MARTENSITIC CLASS AND PREPARATION METHOD THEREOF | 2014 |
|
RU2598725C2 |
HEAT-RESISTANT STEEL OF MARTENSITIC CLASS | 2017 |
|
RU2655496C1 |
REFRACTORY MARTENSITIC STEEL | 2014 |
|
RU2558738C1 |
HEAT-RESISTANT STEEL OF THE MARTENSITIC CLASS | 2020 |
|
RU2757923C1 |
HEAT RESISTANT STEEL OF MARTENSITE CLASS | 2010 |
|
RU2437956C1 |
HEAT-RESISTANT STEEL OF MARTENSITIC CLASS | 2014 |
|
RU2585591C1 |
METHOD FOR PRODUCING WELDED JOINTS OF MARTENSITIC HIGH-CHROMIUM STEEL | 2023 |
|
RU2805532C1 |
Authors
Dates
2014-06-20—Published
2013-03-22—Filed