FIELD: construction.
SUBSTANCE: porcelain mixture contains the following components, pts. wt.: kaolin 28.7-30.8; quartz sand 14.0-16.0; potsherd 1.0-5.0; pegmatite 14.0-16.0; sodium tripolyphosphate 0.2-0.3; vellastonit 14.0-16.0; white-burning clay 20.0-24.0.
EFFECT: increase of the product strength obtained from a ceramic paste.
1 tbl